Specification Temp. (℃) | 1260 | 1260 | 1360 | 1430 | 1600 | |
Working Temp. (℃) | 1050 | 1100 | 1200 | 1350 | 1500 | |
Bulk Density (kg/m3) | 64-160 | 64-160 | 64-160 | 64-160 | 96/128 | |
@24H Linear Shrinkage after Heating | -3 (1000℃) | -3 (1100℃) | -3 (1250℃) | -3 (1350℃) | -1 (1400℃) | |
(w/m.k) Thermal Conductivity | 0.09(400℃) 0.17(800℃) 0.32(1000℃) | 0.09(400℃) 0.17(800℃) 0.31(1000℃) | 0.09(400℃) 0.13(600℃) 0.22(1000℃) | 0.09(400℃) 0.76(600℃) 0.22(1000℃) | 0.16(600℃) 0.28(1000℃) 0.45(1400℃) | |
Tensile strength (MPa) | 0.05 | 0.05 | 0.06 | 0.06 | 0.08 | |
(%) Chemical Composition | Al2O3 | 43 | 44 | 51 | 35 | 71 |
Al2O3+SiO2 | 96 | 98 | 99 | - | - | |
ZrO2 | - | - | - | 13-15 | - | |
Fe2O3 | 1.0 | 0.5 | 0.2 | 0.2 | 0.2 | |
Na2O+K2O | 0.5 | 0.3 | 0.2 | 0.2 | 0.2 | |
Size(mm) | LENGTH*WIDTH*THICKNESS 7200*610/1220*25,3600*610/1220*50,4800*610/1220*38 7200*610/1220*6,14400*610/1220*12.5,28800*610/1220*6.38 | THICKNESS 10-25 |